http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106423259-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-186 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1019 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J29-74 |
filingDate | 2016-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106423259-B |
titleOfInvention | A method of Ag-AgBr/Al-MCM-41 composite functional material is prepared using natural attapulgite |
abstract | The present invention relates to a kind of methods for preparing Ag-AgBr/Al-MCM-41 composite functional material using natural attapulgite, comprising steps of, with inorganic acid soak, obtaining acidification attapulgite using natural clay mineral attapulgite as raw material;It to be acidified attapulgite as raw material, is uniformly mixed with NaOH solid, high-temperature roasting activation;Deionized water is added in attapulgite after activation, takes upper layer leachate spare;The leachate is added in surfactant solution, by the way of assemble in situ, by AgNO 3 It is introduced into above-mentioned synthesis mother liquid, while generating AgBr precipitating, after water-heat process, synthetic product is roasted, obtains composite functional material.The beneficial effects of the present invention are: raw material is cheap and easy to get, preparation process simple possible, utilize assemble in situ method, " synthesis " and " functionalization " step of mesoporous material can be completed, avoid the processes such as the use of solvent and multiple roasting in conventional post treatment method, time-saving energy-saving, and no pollution to the environment. |