http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106423071-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3204 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01P7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-32 |
filingDate | 2016-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106423071-B |
titleOfInvention | A kind of high-ratio surface silkworm excrement porous charcoal MOFs composite material and preparation method and application |
abstract | The invention discloses a kind of high-ratio surface silkworm excrement porous charcoal MOFs composite material and preparation methods and application.First by silkworm excrement and ZnCl 2 It is freeze-dried after solution mixing swelling, silkworm excrement after freeze-drying is carried out to activation reaming reaction in protective gas again, then it cleans again, silkworm excrement base multi-stage porous Carbon Materials are obtained after centrifugation and drying, it is centrifuged after metal salt solution is stirred with the material again, drying, it is passed through oxygen under the conditions of plasma modification and forms high dispersion metal oxide in silkworm excrement base multi-stage porous charcoal material surface, again by microwave irradiation method using high dispersion metal oxide as precursor, MOFs is grown on silkworm excrement base charcoal material surface, it finally filters and dries to obtain high-ratio surface silkworm excrement porous charcoal MOFs composite material.The material can be applied to pesticide and delay controlled release aspect.The obtained carbon composite of present invention specific surface area with higher and carboxylic group, can there is higher adsorption capacity and preferable slow-releasing and controlled-releasing action to pesticide. |