http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106398597-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fa058a43868f5dee60bfc5b1a07050e6
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-001
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-622
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-02
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08
filingDate 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c67391ce37f164efac056f2a5ea86a5b
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9054682517666de049a6bdf94066ce24
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b7309e8cac3a05b9acca5018b992947
publicationDate 2017-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-106398597-A
titleOfInvention Water-based adhesive and its preparation method and battery
abstract The invention provides a water-based adhesive, a preparation method thereof, and a battery. The water-based adhesive includes: a polypropylene emulsion with carboxyl groups; a non-ionic thickener; a conductive agent; a drag-reducing agent; and water. The adhesive does not contain toxic volatile organic solvents, uses water as the medium, is friendly to the physical environment, and is safe for workers. The glue formed by the non-ionic thickener has good stability, and the polypropylene emulsion with carboxyl groups makes the adhesive have Reactivity, good dimensional stability of the electrode after curing.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111263995-A
priorityDate 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104466180-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3028194
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458397365
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID20249141
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419474364
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457707758
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID421305183
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID24261
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6581
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457815232
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559587

Total number of triples: 37.