http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106398316-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2303-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N59-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-80 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01P1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N59-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 |
filingDate | 2016-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106398316-B |
titleOfInvention | A kind of preparation method of the nano zine oxide of doping metals nickel ion |
abstract | A kind of preparation method of the nano zine oxide of doping metals nickel ion is:Take tetra- water nickel acetate of bis- water zinc acetates of 10.56g ~ 9.68g and 0.1592g ~ 1.6979g, it is put into the there-necked flask of 250mL, the analysis ethylene glycol of 70mL is added as solvent, the trisodium citrate of a concentration of 0.058mol/L of 1.2g is as dispersant, above-mentioned solution reacts 4h at 180 DEG C, entire reaction process is always in magnetic agitation, it is carried out under nitrogen protection, obtained sediment is washed three times with absolute ethyl alcohol, each 5min, it washed once with analysis acetone, each 5min, it is washed with deionized again three times, each 5min, ensure that product is a kind of nano zine oxide of pure doping metals nickel ion, product dries 8h in 80 DEG C of vacuum drying chamber.A kind of nano zine oxide of prepared doping metals nickel ion.In ultra violet lamp 50min, it is 91% to reach most degradation rate to methyl orange dye, is up to 19.6mm to the inhibition zone of staphylococcus aureus. |
priorityDate | 2016-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |