http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106391060-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-725 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-0573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-057 |
filingDate | 2016-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106391060-B |
titleOfInvention | A kind of Ag@CdSe/Al2TiO5The preparation method and its usage of composite photo-catalyst |
abstract | The present invention provides a kind of Ag@CdSe/Al 2 TiO 5 The preparation method and its usage of composite photo-catalyst sequentially includes the following steps: step 1, preparation Al 2 TiO 5 Material;Step 2, preparation Ag@CdSe core-shell material;Step 3, preparation Ag@CdSe/Al 2 TiO 5 Composite photo-catalyst.The present invention, which is realized, loads Al with Ag@CdSe 2 TiO 5 For composite photo-catalyst, special catalysis or conversion effet are realized by the interfacial interaction with contaminant molecule, the extremely strong active material of oxidisability is formed by excitation oxygen and hydrone, to achieve the purpose that harmful organic substances in degradation environment. |