http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106391038-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-835 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-835 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-08 |
filingDate | 2016-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106391038-B |
titleOfInvention | A kind of preparation method of spherical shape hierarchical organization stannic oxide/copper oxide composite nano materials |
abstract | The invention belongs to inorganic non-metallic material preparation fields, more particularly to a kind of spherical hierarchical organization stannic oxide/copper oxide composite nano materials preparation method, its with by acetylacetone copper and tin tetrachloride in methanol solution after completely dissolution, carry out solvent thermal reaction, after being filtered, washed, up to spherical hierarchical organization stannic oxide/copper oxide composite nano materials after drying, calcining are cooling.Product of the present invention purity is high, preparation cost is low, and the size of the whole big ball of products obtained therefrom is 3 ~ 6 μm, and the size of nanoparticle is 20 ~ 30 nm, and the homogeneity and good dispersion of product, is easy to be mass produced.Spherical hierarchical organization stannic oxide/copper oxide composite nano materials visible light catalysis activity with higher prepared by the present invention, in degradation of dye waste water and indoor harmful gas, the fields such as photocatalysis disinfection are with a wide range of applications. |
priorityDate | 2016-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.