http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106362760-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-199 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8885 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-888 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C253-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-888 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C255-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C255-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-199 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C253-28 |
filingDate | 2016-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106362760-B |
titleOfInvention | Ammoxidation of aromatic hydrocarbon catalyst, preparation method and its application method |
abstract | The present invention relates to a kind of ammoxidation of aromatic hydrocarbon catalyst, preparation method and its application methods.Mainly solve the problem of that existing ammoxidation of aromatic hydrocarbon catalyst wear-resisting property is poor and is difficult to take into account with catalyst catalytic performance.By preparing by carrier and forming V with the following composition of atomic ratio measuring chemical formula 1.0 Cr a A b B c C d D e E f M g O x Mixed catalyst, wherein A is selected from least one of periodic table of elements group IIIA element;B is selected from least one of the Vth A race of periodic table of elements element;C is selected from least one of alkali or alkaline earth metal element;D is selected from least one of the VIIIth race of periodic table of elements element;E is selected from least one of Mo, Ti, Nb;M is selected from least one of Zr, W;And the technical solution of the preparation method by strict control each component order of addition, the wearability of catalyst is effectively improved, while keeping the high activity selectivity of catalyst, gained catalyst can be applied in the industrialized production of ammoxidation of aromatic hydrocarbon. |
priorityDate | 2016-08-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |