http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106348773-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3886 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-9669 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3865 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3869 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-9607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3217 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-349 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3418 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3427 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-58 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-66 |
filingDate | 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-01-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106348773-B |
titleOfInvention | A kind of anti-lithium electric material erosion fire-clay crucible adding SiAlON-AlN-TiN |
abstract | The invention discloses a kind of anti-lithium electric materials for adding SiAlON-AlN-TiN to corrode fire-clay crucible, it is mixed by weight by following raw material components: 40~80 parts of calcium hexaluminate, 10~30 parts of plate diamond spar fine powder, 10~15 parts of SiAlON-AlN-TiN powder, 3~10 parts of alumina powder, 2~10 parts of silicon powder, 5~10 parts of kaolin, 2~3 parts of waterglass, 1~3 part of methylcellulose, 5~8 parts of water.The present invention produces anti-lithium electric material using the formula and technique of science and corrodes fire-clay crucible, and thermal coefficient is low, and anti-lithium electric material erosion performance is good, and thermal shock resistance is moderate, long service life.Compared with similar crucible, the present invention can protect positive electrode powder and not polluted during the sintering process by crucible material, not occur phenomena such as surface peels off, is scaling-off in service life. |
priorityDate | 2016-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |