http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106207164-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_56b1ec208abfbc296257d94cd889b97e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2015-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_335e6ce902e96d3411988b5937d3d967 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7555156d79a4f48226de80c8affc916 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e92c981f9500945a1909b07415f100f3 |
publicationDate | 2016-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106207164-A |
titleOfInvention | The preparation method of iron manganese phosphate for lithium composite |
abstract | The present invention relates to the preparation method of a kind of iron manganese phosphate for lithium composite.The preparation method of a kind of iron manganese phosphate for lithium composite, it is characterised in that comprise the following steps: by phosphorus-containing compound and the formation soluble in water mixed liquor Han manganese compound;In mixed liquor, add precipitant, after stirring fully precipitation, obtain MnHPO 4 Hydrate, wherein at least one in propanol, isopropanol and butanol of precipitant;By carbon compound and containing at least one in doping element compound, MnHPO 4 Hydrate, lithium-containing compound, it is dried to obtain mixture together with dispersant after ball milling containing ferrous compound;And under the atmosphere of protective gas, mixture is calcined at 550 DEG C~800 DEG C and within 8~16 hours, obtains iron manganese phosphate for lithium composite.Simple and preparation the iron manganese phosphate for lithium composite electrical property of the preparation method technique of above-mentioned iron manganese phosphate for lithium composite is preferable. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115043387-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115043387-B |
priorityDate | 2015-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 110.