http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106189921-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-048 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-08 |
filingDate | 2016-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-01-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-01-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106189921-B |
titleOfInvention | It is a kind of with the POE packaging adhesive films composite tackifier of high bond strength and its application |
abstract | The invention discloses a kind of with the POE packaging adhesive films composite tackifier of high bond strength and its application.Composite tackifier using the present invention can suppress migration of the titanate coupling agent to film surface during adhesive film is cured, and strengthen the combination between silane coupler and titanate coupling agent and glued membrane, by the compound viscosifying action between silane coupler and titanate coupling agent, adhesion strength of the glued membrane to glass and backboard is improved.Wherein, prepare each raw material of packaging adhesive film is included by mass fraction:100 parts of POE resin, 0.4~1.2 part of composite tackifier, 0.8~2 part of crosslinking agent, 0.4~1 part of assistant crosslinking agent, 0.05~0.2 part of ultraviolet absorber, 0.03~0.1 part of antioxidant. |
priorityDate | 2016-08-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |