http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106189016-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 |
filingDate | 2015-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106189016-B |
titleOfInvention | Semiconductive resin composition and power transmission cable using the same |
abstract | An object of the present invention is to provide a semiconductive resin composition having good peelability from an insulating layer and extrusion processability, and a power transmission cable using the same for an outer semiconductive layer. A method for solving the problem is a semiconductive resin composition characterized by comprising: a matrix polymer; two or more of fatty acid zinc, oleic acid bisamide and trimellitate; and a half-life temperature of 1 hour of 130 A peroxide-based crosslinking agent having a temperature of ℃ or higher; and carbon having a DBP adsorption amount of 150 mg/g or less, the matrix polymer containing an ethylene vinyl acetate copolymer having a vinyl acetate content of 60 wt % or more. |
priorityDate | 2014-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.