http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106187799-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C227-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C227-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C229-26 |
filingDate | 2016-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106187799-B |
titleOfInvention | A method of preparing DL-lysine hydrochloride |
abstract | The invention belongs to chemical fields, a kind of method for preparing DL-lysine hydrochloride is disclosed, using L lysine HCL as raw material, deionized water as solvent, raw material L lysine HCL is dissolved in deionized water, in closed container, active carbon decoloring, filters pressing is added in racemization 16~20 hours under 140~155 DEG C of temperature, 0.36~0.54MPa of pressure after reaction in reaction solution, filtrate is concentrated into supersaturation, cooling, crystallization dries and DL-lysine hydrochloric acid product salt is made.The direct racemization of the method for the present invention high temperature and pressure prepares DL-lysine hydrochloride, simplifies separating-purifying step, yield is up to 85% or more, and purity is up to 99.5%.Due to not using inflammable and explosive solvent, so that the input cost of workshop and equipment can be greatly reduced without requirement of explosion proof to workshop and equipment;Replacing organic acid as solvent using deionized water also accordingly reduces environmental protection treatment Capability Requirement. |
priorityDate | 2016-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.