http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106170337-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C67-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-462 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C67-343 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C67-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C69-24 |
filingDate | 2015-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-01-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106170337-B |
titleOfInvention | The method of the active ruthenium catalyst solution for turning vinylation for carboxylic acid is provided |
abstract | The present invention relates to for providing the method for ruthenium catalyst solution, the ruthenium catalyst solution turns to be active, the Ru metal concentration greater than 0.5wt.% comprising the total weight based on ruthenium catalyst solution in vinylation surfactant vinyl esters and surfactant carboxylic acid.The invention is characterised in that a) 70 DEG C to 170 DEG C at a temperature of, at least one ruthenium halide (III) and at least one inorganic or organic base, at least one surfactant vinyl esters and at least one surfactant carboxylic acid reaction;B) molar ratio of surfactant vinyl esters and surfactant carboxylic acid is 1:1.8 to 1.8:1;And c) the total weight based on surfactant vinyl esters and surfactant carboxylic acid, ruthenium halide (III) is used with the amount of the Ru metal of > 0.5wt.%. |