http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106118553-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 |
filingDate | 2016-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106118553-B |
titleOfInvention | A kind of cracking reinforcing agent for wicker products |
abstract | The invention discloses a kind of cracking reinforcing agent for wicker products, including A liquid and B liquid, the A liquid is made of following substance:Wood vinegar, Mancozeb, konjac glucomannan, odium stearate, nonylphenol polyoxyethylene ether, high-carbon fatty alcohol polyoxyethylene ether, positive silicic acid propyl ester, dimethyl silicone polymer, ammonium polyacrylate, boric acid, water;The B liquid is made of following substance:Calgon, tartaric acid, sodium carboxymethylcellulose, active carbon nanoparticles, nano silicon dioxide, propylene glycol methyl ether acetate, acrylic emulsion, phellodendron extract, Camphora extract, water.The cracking reinforcing agent that the present invention prepares is under the collective effect of A liquid and B liquid, it is filled with gap well, avoid erosion of the exogenous impurity ingredient to it, the intensity and wearability of its Vermins-proof mildew-proof performance and entirety are improved again, the surface strength of final wicker products can be improved 40% or so, flexural strength can be improved 50% or so, and service life can extend 1 ~ 2 times, and use value is higher. |