http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106046760-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2463-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2475-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2363-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 |
filingDate | 2016-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106046760-B |
titleOfInvention | The anti-anti-corrosion polyurethane protective film and its preparation method and application that collides with of one kind |
abstract | The invention discloses the anti-anti-corrosion polyurethane protective films and its preparation method and application that collides with of one kind.By weight, prepare raw material includes polyurethane protective film:The thickness of 30~50 parts of thermoplastic polyurethane, 20~30 parts of epoxy resin E44,20~30 parts of epoxy resin E20,40~100 parts of plasticizer, 60~100 parts of filler and 0.2~3 part of corrosion inhibiter, protective film is 2-3mm.In use, the semi-finished product, which are heated to 140 DEG C, again is molten into liquid, it is sprayed at the metal component of surface cleaning, it is cooling, in the protective film for being formed 2-3mm by protection metal component surface.Inventive formulation is simple, of low cost, pollution-free, is particularly suitable for the anti-anti-corrosion protection that collides with of metal product;The present invention manufactures, is easy to use, hand or tool can be used to remove when product unpacking uses, without remaining protective film, the material of stripping can repeatedly use. |
priorityDate | 2016-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |