http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106045363-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 |
filingDate | 2016-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106045363-B |
titleOfInvention | A kind of premixing mortar open hour conditioning agent and preparation method thereof |
abstract | A kind of premixing mortar open hour conditioning agent and preparation method thereof, conditioning agent are made of the raw material of following components and weight proportion:150~400 parts of organic phospho acid or organic phosphonium salt, 150~300 parts of stabilizer raw material, 100~200 parts of magnesium salts, remaining is water;The sum of parts by weight of stabilizer raw material, magnesium salts, water and organic phospho acid or organic phosphonium salt are 1000 parts.Preparation method comprises the technical steps that:Addition polyethyleneimine, hydroxycarboxylic acid (or hydroxycarboxylate) make its mixing in a kettle, add part water, stirring is complete to dissolving, and makes stabilizer;Organic phospho acid or organic phosphonium salt, magnesium salts are added in reaction kettle internal stabilizer, makes its mixing, stirs evenly, be supplemented remaining water, stirring and dissolving to obtain the final product.The present invention has good open hour tuning performance, the arbitrarily open hour of adjustment mortar, the setting time of adjustment time in 10 100h, and develop no big influence for later strength in 6 70h. |
priorityDate | 2016-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |