http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106040117-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2430-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2305-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L31-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K9-1682 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K9-1635 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L31-048 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61K9-1652 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K47-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K9-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K47-32 |
filingDate | 2016-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-05-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-05-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106040117-B |
titleOfInvention | The method that monodispersity calcium alginate microsphere is prepared based on emulsion liquid membrane mass transfer |
abstract | The method that monodispersity calcium alginate microsphere is prepared based on emulsion liquid membrane mass transfer, its processing step are as follows:(1) inner aqueous phase, middle oil phase, outer aqueous phase and the configuration for collecting aqueous phase stream body;(2) respectively by injection-tube, coupling tube and the collecting pipe of inner aqueous phase, middle oil phase and outer aqueous phase fluid injection microfluidic device, form monodispersed water/oil/water lotion, then water/oil/water lotion is introduced into and collected in aqueous phase stream body, and stand at least 2h, collect the Ca in water phase 2+ Reaction generation calcium alginate gel bead is crosslinked into inner aqueous phase and sodium alginate by the oil film mass transfer of water/oil/water double emulsion, while the water in inner aqueous phase enters collection water phase by oil film mass transfer;(3) using collection aqueous phase solution of the filter paper filtering containing calcium alginate microsphere, and washed using deionization, you can obtain the calcium alginate microsphere of monodispersity. |
priorityDate | 2016-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |