abstract |
The present invention provides a sintered alloy having excellent heat resistance and wear resistance, and also having excellent corrosion resistance against salt damage generated in cold regions, and a method for producing the same. In terms of mass ratio, it is composed of Cr: 32.4~48.4%, Mo: 2.9~10.0%, Si: 0.9~2.9%, P: 0.3~1.8%, C: 0.7~3.9%, the balance Fe and inevitable impurities and the carbides are dispersed in the matrix in the form of a density ratio of 90% or more. |