http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105969075-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 |
filingDate | 2016-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105969075-B |
titleOfInvention | Aqueous steel-titanium barrier coating and its application |
abstract | The present invention relates to a kind of coating for preventing from bonding between metal, and in particular to a kind of aqueous steel-titanium barrier coating and its application in titanium ingot preparation process.Aqueous steel-titanium the barrier coating of the present invention, contains following parts by weight ingredient: 50~150 parts of Watery film-fomer, 0~50 part of Cu powder, and Al 2 O 3 400~450 parts of powder, 0~100 part of Fe powder, 300~350 parts of talcum powder.Coating of the present invention can guarantee that titanium tube in 900 DEG C of rollings or perforation procedure, does not occur bonding with steel equipment roll or capstan winch and reacts, and improve the lumber recovery and production efficiency of titanium processing;Simple process, easy to operate, coating is environment friendly and pollution-free, and preparation method is simple. |