http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105883733-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B21-0605 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B21-06 |
filingDate | 2016-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105883733-B |
titleOfInvention | Inflatable carbonitride and preparation method thereof, expansion method |
abstract | Inflatable carbonitride and preparation method thereof, expansion method, it is related to environmental protection, field of fire-proof technology, pass through the method for liquid phase intercalation, it is prepared for inflatable carbonitride, the present invention has synthesized a kind of inflatable carbonitride through sulfuric acid intercalation processing, and the volume after high temperature puffing is handled is changed into original 100 times;The inflatable carbonitride that the present invention is synthesized has an excellent expansion character, great reference area, can further be made as high-performance flame-retardant material, catalysis material, and absorbing material, phase-changing energy storage material and pollutant sorbing material have expanded g C significantly 3 N 4 Application. |