http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105829601-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16G1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16G1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16G5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16G5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-693 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16G1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-693 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-322 |
filingDate | 2014-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105829601-B |
titleOfInvention | It is used to form the aqueous treatment agent of rubber reinforcement cord, using the rubber reinforcement cord and its manufacturing method of its formation and the rubber product for having used the rubber reinforcement cord |
abstract | It is an object of the present invention to improve the anti-characteristic of splitting of rubber reinforcement cord productivity is not greatly lowered.The present invention provides a kind of aqueous treatment agent, it is the aqueous treatment agent for being used to form the rubber reinforcement cord with overlay film, the aqueous treatment agent contains rubber latex, crosslinking agent and packing material, the content of the crosslinking agent is in 50 mass parts or more and 150 ranges below mass part relative to 100 mass parts of solid constituent contained in rubber latex, and the content of the packing material is in more than 50 mass parts relative to 100 mass parts of solid constituent contained in rubber latex and is 80 ranges below mass part. |
priorityDate | 2013-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |