http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105793209-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-26 |
filingDate | 2014-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105793209-B |
titleOfInvention | Method for preparing pozzolan or latent hydraulic cement clinker substitute |
abstract | The present invention relates to a method for preparing a pozzolan or latent hydraulic cement clinker substitute, wherein the temperature is in the range between 500 and 1250°C, preferably between 550 and 1150°C, most preferably between 700 and 900°C The pozzolanic or latent hydraulic cement clinker substitute is formed by calcining the clay using a fuel containing minerals, the resulting mixture of the fuel minerals and the calcined clay, through which the minerals are introduced into the hydraulic cement clinker substitute The ratio is between 1 and 60% by weight. |