http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105778381-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-02 |
filingDate | 2015-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105778381-B |
titleOfInvention | A kind of ACM material, preparation method and applications |
abstract | The invention mainly relates to a kind of ACM material, preparation method and applications.Described ACM material is mainly prepared by the following raw material in parts by weight:90 110 parts of modified active chlorine type acrylate, reinforcing agent 60 85, age resistor 13 and vulcanizing agent 3.3 4.2;Wherein, the ACM material passes through post-cure, and the time of the post-cure is 6 8h.The ACM material processing characteristics of the present invention is excellent, the easy demoulding of product, and use temperature range is wide, it can be used at 35 150 DEG C, lubricating oil resistance energy is good, tensile property loss is small, Volume Changes are small, compression is small, and meet popular PV3307 compression, and cost is low, beneficial to popularization and application. |
priorityDate | 2015-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links