http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105664981-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W10-37 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 |
filingDate | 2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105664981-B |
titleOfInvention | A kind of preparation method of the BiOBr/BiOCl catalysis materials of infrared optical response |
abstract | The present invention relates to a kind of preparation method of the BiOBr/BiOCl catalysis materials of infrared optical response, its step are as follows:1 gram of BiOBr powder is scattered in the hydrochloric acid solution that 40 mL concentration are 0.03 0.08 mol/L, after stirring 15 hours, is centrifuged, washs, drying, you can obtaining the BiOBr/BiOCl catalysis materials of infrared optical response.The preparation method is simple, and obtained composite has excellent infrared photocatalysis performance. |