classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M2101-36 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M13-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C65-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D46-023 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D46-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C65-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-50 |
filingDate | 2016-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-12-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105642034-B |
titleOfInvention | The preparation method and aramid fiber filter bag of aramid fiber filter bag |
abstract | Aramid fiber technical field of the present invention, and in particular to the preparation method and aramid fiber filter bag of a kind of aramid fiber filter bag, methods described are formed, in suture silane coating coupling agent solution, the aramid fiber is aramid fiber 1313 using aramid fiber as fibrous raw material by heat seal process suture.The preparation method of the aramid fiber filter bag of the present invention solves the problems such as existing aramid fiber surface is inert, the weaker, temperature of bonding directly carbonizes decomposition more than 400 DEG C between fiber and fiber at high temperature, obtains the high aramid fiber filter bag of strength, filtering accuracy. |
priorityDate | 2016-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |