http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105603218-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B30-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B30-06 |
filingDate | 2015-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105603218-B |
titleOfInvention | Copper making process bismuth is enriched with the method with recycling |
abstract | The invention discloses a kind of methods of Copper making process bismuth enrichment and recycling.The vulcanized slag that Copper making acid water is handled to the bismuth-containing arsenic generated through high performance vulcanization is added in copper electrolyte, bismuth in vulcanized slag is dissolved in electrolyte and is enriched with, bismuth in electrolyte is adsorbed through efficient selective, desorb, hydrolyze after finally realize recycling in the form of chlorine oxygen bismuth.Method through the invention, the overall recovery of bismuth is up to 90% or more during Copper making.The method of the present invention realizes enrichment and recycling, efficient, the at low cost, environmental protection simple for process of bismuth from source, has good use value. |
priorityDate | 2015-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |