http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105590661-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B13-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 |
filingDate | 2015-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105590661-B |
titleOfInvention | Electrode paste and preparation method thereof |
abstract | The invention discloses a kind of electrode paste, it is prepared from the following raw materials in parts by weight:45~55 parts of electric calcined anthracite or anode scrap block, 45~55 parts of after-smithing petroleum coke, 8~12 parts of asphalt modification resinoid bond, medium temperature coal pitch powder:18~22 parts.The present invention uses normal temperature kneading technique, and kneading is pasted into the block type electrode of definite shape size, then the solvent in vacuum recovery resin, to recycle.Whole technical process is carried out without heating at normal temperatures, so as to solve the problems such as Heavy environmental pollution and energy resource consumption that pitch heating process is brought, while reduces the requirement to production equipment and protection input, has the important value of environmental protection and social effect. |