http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105585977-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J123-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J161-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-16 |
filingDate | 2015-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105585977-B |
titleOfInvention | It is a kind of to improve gluing agent prescription that EPDM rubber is bonded with polyester line and preparation method thereof |
abstract | Gluing agent prescription that EPDM rubber is bonded with polyester line and preparation method thereof is improved the invention discloses a kind of, adhesive Formulation Ingredients mainly include:EPDM elastomeric compounds, phenolic resin, isocyanates, gasoline.EPDM elastomeric compounds are formed by ethylene propylene diene rubber 4045, DCP, sulphur, altax, accelerator TT, zinc oxide ZnO, stearic acid StA, carbon black, white carbon, paraffin oil, anti-aging agent RD mixing.It is 100 by EPDM elastomeric compounds, phenolic resin, isocyanates and gasoline weight ratio:5‑10:0‑3:1000 are made adhesive, can effectively improve the bonding strength of EPDM rubber and polyester line, environmental pollution is small, and preparation technology is simple, practical. |
priorityDate | 2015-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |