http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105565748-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-27 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-06 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-27 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-06 |
filingDate | 2015-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105565748-B |
titleOfInvention | A kind of building marine glue and preparation method thereof |
abstract | The invention discloses a kind of building marine glue, it is made up of according to mass percent 40% 60% A compositions and 40% 60% composition B, A compositions and composition B sum are 100%;A compositions are composed of the following components according to mass percent:Solid polysulfide rubber 5% 15%, marble powder 20% 30%, alumina cement powder 10% 20%, aluminum stearate 20% 30%, vinyl acetate 20% 30%, above component sum is 100%;Composition B is composed of the following components according to mass percent:Styrene-acrylic emulsion 30% 40%, preservative 20% 30%, water 15% 25%, sodium hydrate aqueous solution 15% 25%, above component sum is 100%.The invention also discloses the preparation method of the building marine glue.The building marine glue of the present invention, its adhesive property is good, service life is long, stability is good, and preparation is simple, can meet needs of constructing well. |