http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105561803-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2325-24 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D71-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D71-024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D69-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D67-0046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-444 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D69-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D69-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-44 |
filingDate | 2015-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105561803-B |
titleOfInvention | A kind of big flux, high-precision condensed water in high temperature oil removing remove the preparation method of iron ceramic super-filtering film |
abstract | The invention discloses the preparation method that a kind of big flux, high-precision condensed water in high temperature oil removing remove iron ceramic super-filtering film, including step:1) preparation without silicon alumina ceramic supports:2) preparation of transition tunic:3) preparation of separating layer membrane:Condensed water in high temperature big flux, high-precision ceramic super-filtering film prepared by the present invention, using the alumina ceramic supports without silicon system, silicon dissolution are not had and causes the condensate secondary pollution after processing during use;Condensed water in high temperature prepared by the present invention is high with the high-precision ceramic super-filtering film separation accuracy of big flux, the 50nm of film average pore size 5, membrane flux is big, and water yield is higher than 1.5m3/m2.h, the mg/L of oil content in condensed water in high temperature after processing≤0.3, the μ g/L of the content of iron≤20;Bending strength is more than 8000N, and film heat endurance is more than 800 DEG C. |
priorityDate | 2015-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |