http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105542072-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B24-2652 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-38 |
filingDate | 2016-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105542072-B |
titleOfInvention | A kind of concrete inner curing agent and preparation method thereof suitable for strong alkali environment |
abstract | The present invention provides a kind of concrete inner curing agents suitable for strong alkali environment, are mainly made by following raw material:In terms of mass fraction, 4 12 parts of acrylic compounds, 40 120 parts of acrylamides, 0.05 0.2 parts of crosslinking agent, 0.02 0.10 parts of reducing agent, 0.05 0.2 parts of initiator, 100 300 parts of deionized water.Preparation method includes:After all raw materials are added be mixed evenly successively according to the sequence of deionized water, reducing agent, crosslinking agent, acrylic compounds, acrylamides, initiator, by keeping the temperature, standing, to get concrete inner curing agent after shearing, dry step.The interior curing agent of the embodiment of the present invention is highly suitable for the concrete of strong basicity, strong basicity resisting can be good, water absorbent rate is sufficiently lowered, the size that interior curing agent leaves hole after inside concrete releases water is reduced, does not interfere with the compaction rate and intensity of concrete itself. |