Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J21-185 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2208-00681 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-742 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-162 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8877 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-881 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-882 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8472 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0207 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-745 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-745 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 |
filingDate |
2015-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2017-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2017-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-105517707-B |
titleOfInvention |
The method of CNT aggregate of the manufacture with controllable heap density |
abstract |
The invention provides:It is a kind of to manufacture the loaded catalyst of the CNT aggregate with high heap density;A kind of method for preparing the loaded catalyst;A kind of CNT aggregate obtained by using the loaded catalyst;And a kind of method for manufacturing the CNT aggregate.According to the present invention, the heap density of the CNT aggregate can be easily controlled, accordingly ensure that the application in various fields. |