http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105505195-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6725 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-2815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4825 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6692 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6705 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-348 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 |
filingDate | 2015-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105505195-B |
titleOfInvention | UV-curable waterborne gloss oil and preparation method thereof |
abstract | The present invention relates to a kind of UV-curable waterborne gloss oil and preparation method thereof.The preparation method of UV-curable waterborne gloss oil includes the following steps:Diisocyanate is mixed with dihydric alcohol, reaction obtains the first reaction solution;Dihydroxy carboxylic acids and catalyst are added in the first reaction solution, reaction obtains the second reaction solution, and the second reaction solution and chain extender are mixed, and reaction obtains the 3rd reaction solution;Alkenes end-capping reagent and polymerization inhibitor are added in the 3rd reaction solution, reaction obtains the 4th reaction solution, and triethylamine is added in the 4th reaction solution, and reaction obtains polyurethane acrylate prepolymer;Deionized water is added in polyurethane acrylate prepolymer, emulsion dispersion obtains urethane acrylate dispersoid, urethane acrylate dispersoid, photoinitiator, defoamer and levelling agent are mixed, is dispersed with stirring 15~30 minutes, obtains UV-curable waterborne gloss oil.The UV-curable waterborne gloss oil that the above method is prepared has higher performance. |