http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105492138-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B33Y80-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C1-167 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C1-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C1-162 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B33Y70-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B33Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C9-123 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C9-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-10 |
filingDate | 2014-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105492138-B |
titleOfInvention | The formative method of mold is laminated |
abstract | The stacking formative method that the generation of foul smell can be formed and can effectively inhibited with more easy manufacturing device and the mold for the blocking that will not generate nozzle is used for a long time is provided.It will be covered by water-soluble binder in precoated sand (3) supply to the platform (2) being configured in container-like frame (1) obtained from refractory aggregate, layer of sand (7) is formed by extending component (6) and thinly making its planar development in a manner of becoming certain thickness, then the surface of layer of sand (7) is covered with mask (8), aqueous medium (11) is spread by sprayer (10) to cured part, and then the part for being scattered with aqueous medium (11) of layer of sand (7) is heated by heater (13), to make the mold layer (12) of target shape harden or solidification, the above-mentioned mold layer formation process of number required for repeating, the mold layer sequentially formed (12) is subjected to stacking integration, so as to obtain the stacking mold i.e. molding body (14) of target three-dimensional shape. |
priorityDate | 2013-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |