http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105482111-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-0266 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-02 |
filingDate | 2015-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105482111-B |
titleOfInvention | A kind of PANI/CoFe2O4/Ba0.4Sr0.6TiO3Absorbing material and preparation method |
abstract | A kind of PANI/CoFe 2 O 4 /Ba 0.4 Sr 0.6 TiO 3 Composite granule and preparation method, the present invention is with Ba 0.4 Sr 0.6 TiO 3 Powder and CoFe 2 O 4 Powder is raw material, using the method for In-situ reaction, is induced by ammonium persulfate when aniline forms long chain and CoFe 2 O 4, Ba 0.4 Sr 0.6 TiO 3 Compound, preparation PANI/xCoFe occurs for powder 2 O 4 /(1‑x)Ba 0.4 Sr 0.6 TiO 3 Absorbing material, the present invention prepare trielement composite material PANI/CoFe by in-situ polymerization 2 O 4 /Ba 0.4 Sr 0.6 TiO 3 , improve the absorbing property of absorbing material, reduce match materials thickness, composite wave-suction material is obtained optimum organization to greatest extent, so as to meet that multiband, more mechanism absorb, meet combination property requirement of the modern society to absorbing material. |