http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105481264-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2217-219 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C17-23 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-23 |
filingDate | 2016-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105481264-B |
titleOfInvention | A kind of WO of morphology controllable3The preparation method of film |
abstract | The invention discloses a kind of WO of morphology controllable 3 The preparation method of film.This method is previously deposited one layer of inculating crystal layer using sol-gal process first using sodium tungstate, hydrochloric acid, hydrogen peroxide as raw material on FTO electro-conductive glass;Then WO is prepared using hydro-thermal method as raw material using wolframic acid, sodium tungstate, hydrogen peroxide, hydrochloric acid 3 Film.Synthesis technique of the present invention and required production equipment are simple, it is easy to accomplish industrialized production, it is by changing solvent burden ratio, the WO for the pattern that can be effectively controlled 3 Film. |
priorityDate | 2016-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |