http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105449169-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391 |
filingDate | 2015-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105449169-B |
titleOfInvention | Anode material for lithium-ion batteries, preparation method and lithium ion battery |
abstract | The present invention provides a kind of method for preparing anode material for lithium-ion batteries, and it makes the anode material for lithium-ion batteries of preparation simple, easily controllable with good quasi- single crystal forms, the preparation method technique using the autoclaving crystallization of certain temperature.The formula of anode material for lithium-ion batteries is expressed as Li (Ni made from the preparation method x Co 1‑x‑ y Mn y )O 2 , wherein, 0.34≤x≤0.68,0.15≤y≤0.31,0<x+y<1.The present invention also provides the lithium ion battery containing above-mentioned anode material for lithium-ion batteries. |