titleOfInvention | A kind of method synthesizing cobalt acid nickel spinelle |
abstract | The present invention provides a kind of method synthesizing cobalt acid nickel spinelle, and step is as follows: nickel nitrate, cobalt nitrate and carbamide are joined in deionized water by (1), stirs, make solution mix homogeneously, obtain solution A under room temperature;(2) in solution A, add trihydroxy ethylamine oleate soap, ultrasonic be allowed to mix homogeneously, obtain solution B;(3) solution B is transferred in reactor carry out incubating solvent thermal response, washing, dry, obtain presoma;(4) by presoma in atmosphere after 350 400 DEG C of constant temp. heatings process, cobalt acid nickel spinelle is obtained.The present invention, using deionized water as solvent, with nickel nitrate and cobalt nitrate as reaction raw materials, with trihydroxy ethylamine oleate soap as surfactant, after preparing presoma by solvent-thermal method, and then prepares the big (69m of a kind of specific surface area 2 / g) cobalt acid nickel spinelle, specific capacity is up to 1910F/g, preparation method is simple, product cost is low, be suitable for large-scale production. |