http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105381781-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2220-4806 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2220-42 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N27-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-288 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-0229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-0207 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N27-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-28 |
filingDate | 2015-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105381781-B |
titleOfInvention | A kind of adsorbed film for mixing three kinds of metal oxides and preparation method thereof and the method based on diffusion thin film technique measure fluorine ion |
abstract | The method that fluorine ion in water body and deposit is determined the invention discloses a kind of adsorbed film for mixing three kinds of metal oxides and preparation method thereof and based on diffusion thin film technique (DGT).Wherein three kinds of oxides are dispersed in polyacrylamide solution mainly using three kinds of oxides of iron, aluminium and cerium as sorbing material and form gel, heated gel is prepared into adsorbed film by adsorbed film.The superposition of adsorbed film, diffusion barrier and filter membrane is assembled into DGT devices successively, be positioned in situ detection that fluorine ion can be achieved in water body and deposit and in water and deposit the distribution of fluorine ion sub- centimetre high resolution detection.The adsorbed film adsorption capacity that the present invention is prepared is big, and the holding time is long and sorbing material is easy to get, and compared to traditional fluoride ion selective electrode method, the fluorine ion in-situ detection method based on diffusion thin film technique has a wide range of application, as a result more representative. |