http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105339530-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12896 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01R13-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-505 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01R13-03 |
filingDate | 2014-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105339530-B |
titleOfInvention | Plate the manufacture method and plating material of material |
abstract | The present invention provides a kind of brittle plating material and its manufacture method with excellent wear resistance, electrical conductance, sliding and low frictional properties and suitable for suppression coating.The present invention provides a kind of manufacture method for plating material, it is characterised in that including:First process, has backflow tin coating from least a portion and has at least a portion of the metal base stripping backflow tin coating of conversion zone at the interface of backflow tin coating and metal base;Second process, Nickel Plating Treatment is implemented to having peeled off at least a portion in region of backflow tin coating;3rd process, at least a portion of the nickel coating to being formed by Nickel Plating Treatment implements striking silver-plated process;With the 4th process, silver-plated process is implemented to implementing at least a portion in region of striking silver-plated process. |
priorityDate | 2013-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |