http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105324342-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-087 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-087 |
filingDate | 2014-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105324342-B |
titleOfInvention | Alkali-free glass |
abstract | That the present invention relates to shrinking percentages is low, the mean thermal expansion coefficients at 50 DEG C~350 DEG C are small, is easy to the alkali-free glass of float forming.In particular it relates to a kind of alkali-free glass, the shrinking percentage C1 of the alkali-free glass is 5ppm or less, shrinking percentage C2 is 40ppm hereinafter, in terms of the quality % of oxide benchmark, and the alkali-free glass contains SiO 2 64~72, Al 2 O 3 17~22, MgO 1~8, CaO 4~15.5, and 0.20≤MgO/ (MgO+CaO)≤0.41. |