http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105312055-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-75 |
filingDate | 2015-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105312055-B |
titleOfInvention | A kind of Preparation method and use of type Fenton catalyst |
abstract | The invention provides a kind of Preparation method and use of type Fenton catalyst, including:The step of configuring cobalt nitrate and copper nitrate mixed liquor A;The step of sodium hydroxide solution obtains mixed liquid B is added into mixed liquor A:The step of surfactant obtains mixed liquor C is added into mixed liquid B;The step of mixed liquor C is subjected to incubation water heating reaction;The step of product after hydro-thermal reaction is filtered, washed and is dried in vacuo.Two kinds of metallic elements of cobalt and copper are comprised only in type Fenton catalyst prepared by the present invention, the advantage of catalyst catalytic performance can be improved by taking full advantage of transition metal, and also utilize cobalt and the advantages of copper can widen pH scopes, so that the catalytic degradation performance of the catalyst prepared is good, stability is high, and is respectively provided with preferable catalytic performance in the range of causing catalyst to be 2~10 in pH. |