http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105296690-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C14B1-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C14B1-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C14C11-00 |
filingDate | 2013-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105296690-B |
titleOfInvention | A kind of production method of flexing-resistant leather |
abstract | The present invention relates to leather production technical fields, and in particular to a kind of production method of flexing-resistant leather takes soft cladding, successively by primary coat, boiling hot, middle paintings, top coat, hot light, fall it is bulging to obtain the final product.Wherein, priming step is dissolved in water spray treatment using cationic cerate, acrylic resin;Boiling hot step is boiling hot using cleaning mill;Using leather, then resin is dissolved in spray treatment after water to middle painting step;Top coating step is dissolved in spray treatment after water using acrylic resin isn, acrylic resin JS, leather cracking resin for synthesizing and leather colorant.Method using the present invention, the obtained resistance to complications of leather finish, is not easy trace in use. |
priorityDate | 2013-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links