http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105238169-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2015-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105238169-B |
titleOfInvention | Low-VOC aqueous fluorine carbon metal paint of high durable and preparation method thereof |
abstract | The present invention relates to low-VOC aqueous fluorine carbon metal paint of a kind of high durable and preparation method thereof, the paint is formulated by following components according to following parts by weight:20.6 45.1 parts of water, 0.1 0.4 parts of bactericide, 0.1 0.4 parts of mould inhibitor, 0.2 0.8 parts of dispersant, 0.05 0.35 parts of wetting agent, 0.1 0.6 parts of defoamer, 0.1 0.35 parts of PH conditioning agents, 0.1 0.6 parts of ultra-violet absorber, 7 15 parts of water aluminum-silver slurry, 40 55 parts of water-base fluorocarbon emulsion, 2 4.5 parts of coalescents, 0.4 1 parts of antifreezing agent, 0.2 0.8 parts of freeze thawing resistance surfactant, 0.1 0.5 parts of organosilicon auxiliary agent, 0.5 3 parts of thickener.The paint has zero VOC and superpower weatherability, and the paint can reach the ultraviolet accelerated ageing 1000h of super-fluorescent technical indicator;The preparation method simple and fast, manufacturing cost is low. |
priorityDate | 2015-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |