classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate | 2015-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105219323-B |
titleOfInvention | Castor oil-based polyurethane-acrylonitrile composite emulsion adhesive for leather and preparation method thereof |
abstract | The invention relates to a preparation method of castor oil-based polyurethane-acrylonitrile composite emulsion adhesive for leather. Its preparation method is: mix 10wt%~20wt% castor oil, 30wt%~40wt% polytetrahydrofuran ether glycol, 10wt%~30wt% diisocyanate and 0wt%~5wt% catalyst, under N2 gas and 50 ℃~100℃ for 1~6h, then add 4wt%~8wt% dimethylol fatty acid, react for 1h~6h under 50℃~100℃, then add 3wt%~6wt% triethylamine And, then add a sufficient amount of deionized water and stir at 3000r/min to obtain a polyurethane emulsion with a solid content of 40%, and then add 10wt% to 20wt% of acrylonitrile and 1wt% to 6wt% to the prepared polyurethane emulsion The initiator is reacted at 50°C-100°C for 1h-6h to prepare castor oil-based polyurethane-acrylonitrile composite emulsion adhesive. The invention is an effective method for preparing environment-friendly emulsion adhesive by utilizing renewable resources. |
priorityDate | 2015-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 45.