http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105176042-B
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-372 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-132 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3475 |
filingDate | 2015-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105176042-B |
titleOfInvention | A kind of anti-fog properties good resin lens and preparation method thereof |
abstract | The present invention relates to a kind of anti-fog properties good resin lens and preparation method thereof, wherein raw material includes 40~50 parts of Merlon, 15~20 parts of allyl etherization phenolic resin, 15~20 parts of four mercaptoacetate of tetramethylolmethane, hexa-methylene 1,6 8~10 parts of diisocyanate, 15~20 parts of cellulose nitrate, 3~5 parts of propenyl, 2~4 parts of UV absorbent, 3~5 parts of coupling agent, 0.5~1.5 part of catalyst, 0.5~1.5 part of releasing agent, raw material can be made through cured, the demoulding, trimming, cleaning eyeglass is obtained.Present invention can ensure that while prepared resin lens have excellent refractive index and light transmittance, the anti-fog performance of resin lens can be greatly improved, be conducive to improving the comfortableness of glasses. |
priorityDate | 2015-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |