abstract |
The present invention provides a composition containing 1,2-alkane polyol with 4 to 18 carbon atoms as the alkane polyol, wherein 1,2-alkane polyol with 4 to 18 carbon atoms is poor in chemical stability and easily deteriorates. , The time-dependent deterioration of the 2-paraffin polyol is suppressed, and the composition can be suitably used for coating materials such as cosmetics, inkjet inks, fibers, and paints. A composition containing 1,2-alkane polyol, which is a composition used for cosmetics, inkjet inks, fiber raw materials or coating materials, and containing 1,2-alkane polyol, the above-mentioned chain The alkane polyol is a 1,2-alkane polyol with 4 to 18 carbon atoms, and the composition contains a free radical scavenger. |