http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105132630-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C7-076 |
filingDate | 2015-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105132630-B |
titleOfInvention | It is a kind of to be used for electric furnace, composite slag lotion of converter and preparation method thereof |
abstract | It is used for electric furnace, composite slag lotion of converter and preparation method thereof the invention provides a kind of, belongs to metallurgic auxiliary materials technical field.It is a kind of to be used for electric furnace, the composite slag lotion of converter, include the active ingredient of following weight/mass percentage composition:Calcium oxide:30 ~ 50%, alundum (Al2O3):20 ~ 40%, barium monoxide:5 ~ 20%, magnesia:3 ~ 15%, reducing agent:5~15%.The combination property of product wash heat agent of the present invention is protruded, and has not only improved deoxidation, desulfurization and the dephosphorization effect of existing wash heat agent, and substantially shortens the LF refining time, is mingled with ability with good absorption, to smelting molten steel without introducing impurity;In addition, raw material type and reasonable mixture ratio so that the cost of product of the present invention is substantially reduced than existing dephosphorized slag lotion, with the obvious market advantage. |