classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 |
filingDate | 2014-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-05-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-05-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105111882-B |
titleOfInvention | Light-resistant antibacterial water-based acrylic resin coating used in building industry |
abstract | The invention relates to a light-resistant antibacterial water-based acrylic resin coating used in building industry. The preparation method comprises the following steps: adding water, an emulgator and acrylic acid; heating till the temperature reaches 45 DEG C; stirring for 45 min; adding an A monomer, an antibacterial material and cationic polyacrylamide; carrying out emulsification for 40-60 min; heating till the temperature reaches 80 DEG C and keeping the temperature; dropwise adding an initiator B for 0.5-2.5 h; after addition, reacting for 2 h to obtain a nuclear layer emulsion; dropwise adding a monomer C and an initiator C into the nuclear layer emulsion for 1-3 h at the same time; after addition, keeping the temperature of 75-85 DEG C for reaction for 2 h; adding polyaniline and dodecyloxy benzoic acid; adjusting the pH to be 4 by using hydrochloric acid; keeping the temperature of 75-85 DEG C for reaction for 1-3 h; adding metal salt; adjusting the pH to be 4.0; keeping the temperature of 75-85 DEG C for reaction for 1-2 h; cooling till the temperature reaches 50 DEG C; adding a cross-linking agent for reaction for 30 min; adding ammonia water; adjusting the pH to be 5; adding p-dodecylbenzenesulfonyl chloride; adjusting the temperature to be 75-85 DEG C; reacting for 30 min to obtain the light-resistant antibacterial water-based acrylic resin coating. |