http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105086157-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-062 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 |
filingDate | 2015-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-105086157-B |
titleOfInvention | A kind of automotive upholstery Antistatic anti-aging plastic and preparation method thereof |
abstract | The invention discloses a kind of automotive upholstery Antistatic anti-aging plastic, it is made up of the raw material of following parts by weight:5 ~ 12 parts of 40 ~ 65 parts of acrylic resin, 38 ~ 55 parts of high-density polyethylene resin, POE20 ~ 35 part, 5 ~ 20 parts of Polyethylene Glycol Oleate, 6 ~ 18 parts of ALS, 8 ~ 20 parts of chlorinated paraffin, 4 ~ 16 parts of glass fibre, 3 ~ 22 parts of pentaerythritol stearate, 5 ~ 17 parts of ethylene methacrylic acid ethylene oxidic ester, 7 ~ 15 parts of brucite powder, 3 ~ 19 parts of calcium sulfate, 6 ~ 13 parts of carborundum, 5 ~ 16 parts of barium stearate, 2 ~ 8 parts of fire retardant and composite antioxidant.Automotive upholstery Antistatic anti-aging plastic prepared by the present invention, test result show higher specific insulation, illustrate that the antistatic effect of prepared material is good.In addition, after air aging 500h at 120 DEG C, the stretching strength retentivity and impact strength conservation rate of prepared material are above 84.7%, and the material prepared by this explanation present invention also possesses good antioxygenic property. |